Composition %
Nichel - 34.5 - 41.0 | |
---|---|
Fier - resturi | |
Crom - 17.0 - 19.0 | |
Siliciu - 1.90 - 2.60 | |
Carbon - max. 0.10 | |
Mangan - 0.80 - 1.50 | |
Cupru - max. 0.50 | |
Titan - max.0.20 | |
Sulf - max.0.03 |
General properties
Alloy DS / Incoloy DS ® (W-Nr. 1.4862)
A nickel-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospheres. The alloy’s austenitic microstructure remains stable during long-time exposure to high temperature.
Used in industrial heating for furnance muffles, retorts, and conveyor systems and for heat-treating baskets and fixtures.